FindTestingLabs
Registers refreshed 2026-11-06.See refresh dates

ASTM D6110 Accredited Testing Labs Worldwide

11 accredited laboratories in 2 countries hold ASTM D6110 in their ISO/IEC 17025 scope. Primary accreditors include American Association for Laboratory Accreditation. In the register, ASTM D6110 scope entries most often cover Aluminum, Fogging, Notch Depth in Plastics.

Total labs
11
Countries
2
Top matrix
Plastics
3 labs

Available in 2 Countries

Top matrices for ASTM D6110

Top analytes for ASTM D6110

  • Aluminum (1)
  • Fogging (1)
  • Notch Depth (1)

Sample labs

Element Materials Technology Anaheim
Anaheim, CA, US

ASTM D6110 Ionic Cleanliness - Conductivity IPC-A-600; IPC-4202; IPC-6012; IPC-TM-650 (Methods 2.3.25.1 and 2.3.25); MIL-P-50884 2; MIL-PRF-50884 2; MIL-PRF-31032 2; MIL-PRF-55110 2 Mass and Thickness (Reusable Bags) ANA-0024

DatapointLabs
Ithaca, NY, US

ASTM D6110 ASTM E8/E8M ASTM E112 ASTM E1251 Coefficient of Linear Thermal Expansion of Solid Materials by Thermomechanical Analysis ASTM E831 Rubber – Determination of Tensile Stress-Strain Properties ISO 37 Determinatio

Element Broken Arrow
Broken Arrow, OK, US

Test Test Method(s) Metallographic Evaluation (cont’d) Microhardness Knoop (100 to1000) gf ASTM B578, E92, E384, F606/F606M; NASM 1312-6; NAVSEA S9074-GIB-010/248 Vickers (100 to 1000) gf ASTM B578, E92, E384, F606/F60

Element Los Angeles
Duarte, CA, US

ASTM D6110 Test Method for Determining th e Charpy Impact Resistance of Notched Specimens of Plastics ASTM D6264 Test Method for Measuring the Damage Resistance of a Fibe r-Reinforced Polymer-Matrix Composite to a Concentrated Quasi-S

Chemitox, Inc., Yamanashi Testing Center KAI
Yamanashi-ken 408-0103, JP

ASTM D6110; JIS K7111-1, JIS K6911 (Section 5.20); ISO 179-1; UL746A (Section 15); CSA C22 No.17 (Section 5.2) Heat Deflection Temperature (HDT) UL746A; ASTM D648; ISO 75-1, 75-2; JIS K7191-1, JIS K7191-2 Vica

Ghesquiere Plastic Testing
Harper Woods, MI, US

ASTM D6110; DIN 53453; GMW14093, ISO 179, ISO 180; Rivian RTS.1776; Toyota TSM 0501G

Intertek Testing Services NA
Kentwood, MI, US

Test(s): Test Method(s) 1: Peel Strength ASTM D903, D3330/D3330M Pendulum Impact ASTM D256, D4812, D6110; ISO 179-1, 180 Shear ASTM C273 / C273M, D732, D2344 Slow Rate Puncture ASTM F1306; MIL STD 3010 Tea

Elite Electronic Engineering
Downers Grove, IL, US

ASTM D6110; FAA AC 150/5345-42 Accelerated Life Test FAA AC 150/5345-46; FAA EB-67 Humidity 2 (5 to 95) %RH MIL-STD-810 (C/E/F/G/H), Methods 507 and 520; MIL-STD-202 (F/G/H), Methods 103 and 106; SAE J1455, Sections 4.2 and 4.1

Architectural Testing, Inc. (An Intertek Company)- York
York, PA, US

ASTM D6110 Standard test method for determining the Charpy impact resistance of notched specimens of plastics ASTM D6511/D6511M Standard Test Methods for Solvent Bearing Bituminous Compounds (section 7 only) ASTM D6662 Standard specific

Westmoreland Mechanical Testing & Research
Youngstown, PA, US

Building AP14 Test: Test Method(s): Non-Metallic Materials Testing Specimen Preparation of Composite Materials ASTM D5687/D5687M Specimen Conditioning ASTM D5229, EN 3615 Mechanical Properties Charpy / IZOD Impact ASTM D2

Riverview Calibration Services,
Belpre, OH, US

IV. Plastic Industry: Specific Measurements Parameter/Equipment Range CMC2 (±) Comments Verification of Izod or Charpy Notch Depth – Radius Angle Depth Up to 0.5 in (15 to 45)° (0.001 to 0.5) in