Metaltech Services
Gateshead, GB
ASTM E18-24 GAT Vickers (Hv10) BS EN ISO 6507-1:2023 ASTM E92-23 GAT Vickers Micro / Low force (Hv0.3, 0.5 & Hv1.0) BS EN ISO 6507-1:2023 ASTM E384-22 GAT Impact: Charpy at -80°C to ambient temperature
34 laboratories in United Kingdom are accredited to perform ASTM E18 testing, 31 of them by UKAS. We don't know yet whether 11 of them take outside work. From the accredited scope text: “ASTM E18 MID Vickers (HV5, HV10 & HV30) BS EN ISO 6507-1 ASTM E92 MID Vickers Hardness (Low Force and Microhardness) (HV0.1, HV0.2 and HV0.5) BS EN ISO 6507-1 ASTM E92 ASTM E384 MID Proof loading: Bea” “ASTM E18-24 Tensile Tensile-Ambient Temperature (Forces up to 100 KN) BS EN ISO 6892-1:2019 Method A ASTM E8/E8M-24 Tensile (Elevated Temperatures in range 400 to 1100 ºC) (Forces up to 100 KN) BS EN” “ASTM E18-24 Vickers (HV 0.3, 5, 10, 30) BS EN ISO 6507-1:2023 ASTM E384-22 ASTM E92-23 Impact:- Charpy (-196 °C and -120 °C to ambient temperature) Including lateral expansion and percentage shear by” “ASTM E18:24 A Impact: Charpy (V- Notches) (-196°C to 80°C) ASTM E23-24 ASTM A370-24a A”
Gateshead, GB
ASTM E18-24 GAT Vickers (Hv10) BS EN ISO 6507-1:2023 ASTM E92-23 GAT Vickers Micro / Low force (Hv0.3, 0.5 & Hv1.0) BS EN ISO 6507-1:2023 ASTM E384-22 GAT Impact: Charpy at -80°C to ambient temperature
Wolverhampton, GB
ASTM E18 END
Hereford, GB
ASTM E18-24
County Durham, GB
ASTM E18 CON Vickers (HV5, 10 & 30) BS EN ISO 6507-1 ASTM E92 CON Vickers – Micro (HV0.2) BS EN ISO 6507-1 ASTM E384 CON Impact: Charpy at -196°C and -120°C to ambient temperature including % shear and l
Norfolk, GB
ASTM E18 Vickers (HV5, 10) BS EN ISO 6507-1 ASTM E92 Tensile at ambient temperature (Forces up to 600 kN) BS EN ISO 6892-1 ASTM E8/E8 ASTM A370 ASTM B557 Impact testing: Charpy (-196°C and -123°C to Am
Banbury, GB
ASTM E18 Vickers Hardness (HV5, HV10, HV30) ASTM E92
Oldham, GB
ASTM E18-24 ASTM A370-24a A Impact: Charpy (temperatures from -196 °C and -120 °C to ambient) BS EN ISO 148-1:2016 ASTM E23-23a ASTM A370-24a ASTM A923-23 (Method B) A Through thickness tensile BS EN 10164:2018
Sheffield, GB
ASTM E18-22 Vickers (HV10 & HV30) BS EN ISO 6507-1:2023 ASTM E92-23 Corrosion Resistance to pitting corrosion ASTM G48-11(2020) (Method A) Inter-granular corrosion ASTM A262-15 Practice E(2021) ASTM G28- 22 Method
Sheffield, GB
ASTM E18:2024 Metallurgical tests Grain size determination ASTM E112:2024 Inclusion content ASTM E45:2018a Method A Stainless steels Determination of intergranular attack ASTM A262:2021 Practice A Corr
South Yorkshire, GB
ASTM E18 Vickers ( HV10 and HV30) BS EN ISO 6507-1 ASTM E92 Vickers Micro-hardness (HV0.3, HV0.5 and HV1.0) BS EN ISO 6507-1 ASTM E384 Impact: Izod BS 131:Part 1 Charpy (V and U notches) (temperatures, -
West Midlands, GB
ASTM E18-24 A Vickers HV5, HV10, HV30 BS EN ISO 6507-1:2023 ASTM E92-23 A Vickers HV10 BS EN ISO 6507-1:2023 ASTM E92-23 B Low Force Vickers HV0.3, 0.5 and 1 BS EN ISO 6507-1:2023 A Micro Hardnes
West Yorkshire, GB
ASTM E18 Bend BS EN ISO 7438 ASTM E290 Shear BS EN 28749
Burton on Trent, GB
ASTM E18-24 Impact: Charpy at -196°C and -80°C to ambient temperature (Including lateral expansion & shear) ASTM E23- 25 ASTM A923-23 Method B ASTM A370-24a Tensile: Ambient Temperature (Forces from 6kN to
South Yorkshire, GB
ASTM E18-24 ASTM A370-24a Vickers (HV10 & HV30) BS EN ISO 6507-1:2023 Metallurgical Tests Grain size (Comparison & Linear Intercept Methods) ASTM E112-24 BS EN ISO 643:2024 ASTM E1181-02(2023) ISO 14520: 2000 AST
Wolverhampton, GB
ASTM E18- 24 Impact: Charpy at -101°C to ambient & -196°C (including % Shear & Lateral Expansion) ASTM E23- 24 BS EN ISO 148-1 :2016 Tensile: Ambient Temperature (Forces from 2kN to 600kN) BS EN ISO 689
Derbyshire, GB
ASTM E18-22 B Tensile: Tensile (ambient temperature) (Force from 0.4kN to 1000kN) BS EN ISO 6892-1:19 BS EN 2002-1:2005 BS 4A4:Part 1:Section 1:1966 (Withdrawn) ASTM A370-24a ASTM E8/E8M-25 B Tensile (elevated
Abingdon, GB
ASTM E18-24 Vickers (HV5, 10 and 30) BS EN ISO 6507-1:2023 ASTM E92-23 Impact: Charpy (V- notch) (-196°C and -50°C to Ambient Temperature) BS EN ISO 148-1:2016 Percentage shear Lateral Expansion BS EN ISO 148-
West Midlands, GB
ASTM E18-24 Vickers (HV 0.3, 5, 10, 30) BS EN ISO 6507-1:2023 ASTM E384-22 ASTM E92-23 Impact:- Charpy (-196 °C and -120 °C to ambient temperature) Including lateral expansion and percentage shear by comparison
Lancaster, GB
ASTM E18 MID Vickers (HV5, HV10 & HV30) BS EN ISO 6507-1 ASTM E92 MID Vickers Hardness (Low Force and Microhardness) (HV0.1, HV0.2 and HV0.5) BS EN ISO 6507-1 ASTM E92 ASTM E384 MID Proof loading: Bear
West Midlands, GB
ASTM E18-24 Vickers Hardness HV10 BS EN ISO 6507-1:2023 ASTM E92-23 Impact: Charpy V-notch (-196°C and -85°C to Ambient) BS EN ISO 148-1:2016 ASTM E23-25 ASTM A370-24a Tensile: Ambient Temperature (
Biggleswade, GB
ASTM E18-24 Main Lab Vickers (HV10, 30) BS EN ISO 6507-1:2023 ASTM E92-23 Main Lab Brinell (HBW 10/3000) BS EN ISO 6506-1:2014 ASTM E10-23 Main Lab Impact Charpy V notch including % shear and latera
West Midlands, GB
ASTM E18-24 Vickers (HV10) BS EN ISO 6507-1:2023 Low load Hardness (Vickers HV0.5) BS EN ISO 6507-1:2023 ASTM E384-22
West Midlands, GB
ASTM E18-24 Vickers Hardness (micro indentation) BS EN ISO 6507-1 :2018 ASTM E92-23 ASTM E384-22 Determination of decarburisation and carburisation ASTM F2328/F2328-17(2022) Macroetch testing for steel and alloy AST
Leicester, GB
ASTM E18-24 Titanium alloy fasteners Chemical Analysis: - Hydrogen determination Documented In-House Method Laboratory Instruction LI 16 Titanium alloys Low alloy steels Stainless steels Ni-base alloys Metallog
Derbyshire, GB
ASTM E18-22 END
South Yorkshire, GB
ASTM E18-24 Vickers (HV10 & HV30) BS EN ISO 6507-1:2023 ASTM E92-23 END
Sheffield, GB
ASTM E18:24 A Impact: Charpy (V- Notches) (-196°C to 80°C) ASTM E23-24 ASTM A370-24a A
West Yorkshire, GB
ASTM E18-24 Tensile Tensile-Ambient Temperature (Forces up to 100 KN) BS EN ISO 6892-1:2019 Method A ASTM E8/E8M-24 Tensile (Elevated Temperatures in range 400 to 1100 ºC) (Forces up to 100 KN) BS EN ISO 6892-2 :2018
Leeds, GB
ASTM E18, ASTM F606/F606M; ISO 898-1, ISO 898-2, ISO 6508-1 Tensile (Axial, Wedge) ASTM A370, ASTM F606/F606M; ISO 898-1, ISO 3506-1 Proof (Internal/External Threaded) Bolts Nuts ASTM A370, ASTM F606/F606M; ISO 89
Dorset, GB
ASTM E18 indirect method GRE Scales & Balances3 Up to 230 g (230 to 1200) g (1200 to 6200) g (6200 to 34 000) g 0.51 mg 0.00 13 % - 0.42 mg 0.00 14 % + 7.4 mg 0.00 46 % + 210 mg ASTM Class 1 weights CLW, P
Wolverhampton, GB
ASTM E18-24 Vickers (HV0.5 and 0.3) BS EN ISO 6507-1:2023 ASTM E384-22 ASTM E92-23 Knoop (HK0.5 and 0.2) BS EN ISO 4545-1:2023 ASTM E384-22 ASTM E92-23 Impact Charpy at -196°C and -101°C to ambient temperature incl
Devon, GB
ASTM E18-24 Stress Rupture (700°C -1050°C) BS EN 2002-005:2007 ASTM E139-11(2018) BS EN ISO 204:2023 Tensile tests Ambient Temperature (Range 0.1 - 50kN) Elevated Temperature (650 °C and 850 °C) Excluding
Sheffield, GB
ASTM E18-22 Vickers (HV10 & HV30) BS EN ISO 6507-1:2023 ASTM E92-23 Brinell (HB 10/3000) BS EN ISO 6506-1:2014 ASTM E10-23
South Yorkshire, GB
ASTM E18-24 RRMS 30038 Rev B A Rockwell (Scale B & C) BS EN ISO 6508-1:2023 ASTM E18-24 B Vickers (HV10 & 30) BS EN ISO 6507-1:2023 RRMS 30038 Rev B A Vickers (HV10 & 30) BS EN ISO 6507-1:2023 B Vickers M
United Kingdom Accreditation Service (UKAS) is the primary accreditation body issuing ISO/IEC 17025 accreditation for testing laboratories in United Kingdom.
ISO/IEC 17025 is the international standard for the competence of testing and calibration laboratories. Accreditation to this standard provides independent confirmation that a laboratory operates a quality management system and is technically competent to produce valid results within its declared scope.