Technical Maintenance, Inc. - PEACHTREE CORNERS
Peachtree Corners, GA, US
ASTM E92 Indirect Verification of Microindentation Vickers3 (100 to 1000) HV (12 + 0.012X) HV ASTM E92 Indirect Verification of Hardness Brinell 10mm ball HBW 500kg 1000 kg
99 laboratories in United States are accredited by A2LA to perform ASTM E92 testing. We don't know yet whether 22 of them take outside work. From the accredited scope text: “ASTM E92 using NIST Vickers or Knoop standard reference material (SRM) 1906, 1893, 1894a, 1895, and 1896. All other micro-indentation scales are traceable to the MPA or Sun-Tec hardness levels through” “ASTM E92 ASTM E112 Vickers and Knoop Hardness of Metallic Materials Avera ge Grain Size (Comparison Procedure & Intercept Method) ASTM E290 Bend Testin g (except Guided Bend) ASTM E313 Yellowness Inde” “ASTM E92 Microhardness1: Knoop (25, 50, 100, 200, 500, 1000gf) ASTM E92/E384; NASM-1312-6 Vickers (10, 25, 50, 100, 200, 300, 500, 1000gf) ASTM E92/E384; NASM-1312-6 Metallographic Examination1: Prepa” “ASTM E92; NACE MR0175/ISO 15156 Proof Load ASTM A370, F606/F606M; SAE J429, J995 Charpy, V-notch Impact ASTM A370, E23 Bend Test ASTM A370, E190, E290 Flattening ASTM A370, API 1104 Nick Break API 110”
Peachtree Corners, GA, US
ASTM E92 Indirect Verification of Microindentation Vickers3 (100 to 1000) HV (12 + 0.012X) HV ASTM E92 Indirect Verification of Hardness Brinell 10mm ball HBW 500kg 1000 kg
Colorado Springs, CO, US
ASTM E92 Indirect Verification of Microindentation Vickers3 (100 to 1000) HV (12 + 0.012X) HV ASTM E92 Indirect Verification of Hardness Brinell 10mm ball HBW 500kg 1000 kg
Euless, TX, US
ASTM E92 Brinell Hardness (500 and 3000) kgf ASTM E10, ASTM E110 Rockwell Hardness (A, B, C, E, 15N, 30N, 45N, 15T, 30T, 45T) ASTM E18, ASTM F3125 Leeb Portable Hardness1 ASTM A956 Weld Operator and Weld Procedure Qualificati
Kennesaw, GA, US
ASTM E92, ISO 6507-2 Verification of forces by an Load cell Stage micrometer Stopwatch US Indirect Verification of Brinell Hardness Testers at Test Conditions 3 – 10/3000 5/750
Houston, TX, US
ASTM E92, ASTM E384 ASTM E92, ASTM E384; ISO 15614-1, ISO 9015-1, ISO 9015-2, 15156-1, ISO 6507 Magnetic Permeability ASTM A342/A342M; MIL-I-17214
Decatur, TX, US
ASTM E92; ASTM E140; ARP 1820 Porosity AMS-QQ-C-320; AMS 2460; AMS 2438; ASTM B733; AMS-P-81728; MIS 41177 Salt Spray Corrosion ASTM B117 Solderability ASTM B678; QQ-S-365 Taber Abrasion ASTM D4060; ASTM B1023; FED-STD-141
Fairview, TN, US
ASTM E92
Milwaukee, WI, US
ASTM E92, F606/606M Impact (V-notch and U-notch) -320 °F, -150° F to RT ASTM E23, A370; DIN 10045-1(Withdrawn 2010)*; ISO 148-1; JIS-Z-2242 Metallographic Evaluation: Case Depth SAE J423 Depth of Decarburization (M
Wixom, MI, US
ASTM E92, ASTM E384 Microhardness Knoop / Vickers (Automated Up to 1 kg) ASTM E384 Metallographic Evaluation Sample Preparation ASTM E3 Case Depth SAE J423 Grain Size ASTM E112, ASTM E930, ASTM E1181 Inclusion Ratings by Im
Temple Terrace, FL, US
ASTM E92 Indirect Verification of Microindentation Vickers3 (100 to 1000) HV (12 + 0.012X) HV ASTM E92 Indirect Verification of Hardness Brinell 10mm ball HBW 500kg 1000 kg
Portland, OR, US
ASTM E92, E384; SAE ARP 1820 Knoop (300, 500) g Vickers (100, 300, 500, and 10,000) g
Daleville, IN, US
ASTM E92, ASTM E384; NASM 1312-6; ISO 6507-1 Knoop (25, 50, 100, 200, 300, 500, 1000g) ASTM B578, ASTM E92, ASTM E384; NASM 1312-6; ISO 6507-1 Hydrogen Embrittlement ASTM F519 Impact Testing Charpy Impact (-150 - 100) °F
Naperville, IL, US
ASTM E92, ISO 6507-2 Stage micrometer
Windsor, CT, US
ASTM E92 Indirect Verification of Microindentation Vickers3 (100 to 1000) HV (12 + 0.012X) HV ASTM E92 Indirect Verification of Hardness Brinell 10mm ball HBW 500kg 1000 kg
Broken Arrow, OK, US
ASTM E92, F606/F606M Charpy Impact (-325 to 80) °F (U- and V- Notch) ASTM A370 (Section 20-27), E23, A923; ISO 148-1 Flattening API 1104; ASTM A370 (Section A.2.5.1.1); A530/A530M (Section 21), A1016/A1016M (Section 19), A999/A9
San Carlos, CA, US
ASTM E92 Indirect Verification of Microindentation Vickers3 (100 to 1000) HV (12 + 0.012X) HV ASTM E92 Indirect Verification of Hardness Brinell 10mm ball HBW 500kg 1000 kg
St. Louis, MO, US
ASTM E92 ASTM A956
Charlotte, NC, US
ASTM E92 with test blocks Indirect Verification of Rockwell Hardness Testers 3 HRC: Low Medium High HRBW: Low Medium High 1 HRC 1 HRC 1 HRC 1 HRBW 1 HRBW 1 HRBW Indi
New Iberia, LA, US
ASTM E92; ASTM E384; BS EN ISO 9015-1; ISO 6507-1 Impact, Charpy V-Notch (-321 to +212) °F ASTM A370, A923 (Method B), E23; BS EN ISO 9016; ISO 148-1 Nick – Break Testing API 1104 Metallography (Micro) Preparation
HOMEWOOD, AL, US
SCOPE OF ACCREDITATION TO ISO/IEC 17025:2017 VISTA ENGINEERING & CONSULTING LLC 130 Citation Court Homewood, AL 35209 Amanda Reagan Phone: 205 532 1250 Email: areagan@vistaeng.com MECHANICAL Valid To: September 30, 2027
Cleveland, OH, US
ASTM E92, E384, F606/F606M; NASM 1312-6; ISO 6507, ISO 898-5 (6.1.1) Shackles RR-C-271 Tape Adhesion ASTM D3359; FED-SPEC-141C Twist Test ASTM A938, ISO 7800 Wrap Test ASTM A370 (A4.7) Evaluation of the Degree of Blistering of Pa
Ithaca, NY, US
ASTM E92 ASTM E112 Vickers and Knoop Hardness of Metallic Materials Avera ge Grain Size (Comparison Procedure & Intercept Method) ASTM E290 Bend Testin g (except Guided Bend) ASTM E313 Yellowness Index ASTM E340 Macroetchin g Meta
Aurora, IL, US
ASTM E92 Load cell Line scale Stopwatch Chicago
Nicholasville, KY, US
Parameter/Equipment Range CMC2, 4, 7 (±) Comments Indirect Verification of Rockwell Hardness Testers3 HRA: Low Medium High HRBW: Low Medium High HRC: Low Medium High 15N: Low Mediu
Whitmore Lake, MI, US
ASTM E92 Microhardness Vickers (200, 300, 500 and 1000) gf Knoop (200, 300, 500) gf ASTM E384; ISO 15614-1 Metallographic Evaluation Sample Preparation ASTM E3 Case Depth SAE J423 Depth of De
Columbia City, IN, US
Parameter/Equipment Range CMC2, 5, 10 (±) Comments Indirect Verification of Rockwell Hardness Testers3 (cont) HR45T: Low Medium High 1.3 HR45T 1.3 HR45T 1.2 HR45T Indirect verification per ASTM E18 In
Dallas, TX, US
ASTM E92 Indirect Verification of Microindentation Vickers3 (100 to 1000) HV (12 + 0.012X) HV ASTM E92 Indirect Verification of Hardness Brinell 10mm ball HBW 500kg 1000 kg
Livonia, MI, US
ASTM E92 Metallographic Analysis Case Depth Cast Iron Rating Depth of Decarburization Grain Size Inclusion Content Macroetching Microetch SAE J423 ASTM A247; SAE J158, J434 ASTM E1077; SAE J419 ASTM E112 (Comparison Only) AST
Marietta, GA, US
Parameter/Equipment Range CMC2 (±) Comments Indirect Verification of Rockwell Hardness & Rockwell Superficial Hardness Tester3 (cont) HR45N: Low Medium High HR45TW: Low Medium High HR45YW: Low High
Lakeside, CA, US
SCOPE OF ACCREDITATION TO ISO/IEC 17025:2017 EXPEDITE TESTING SERVICE CORPORATION 11645 Riverside Dr. #127 Lakeside, CA 92040 Tiffany Arnold Phone: (619) 736 - 7872 E-mail: tiffanya@expeditetest.com MECHANICAL Valid
Irving, TX, US
ASTM E92 Hardness Testers – Knoop, Indirect Verification 3 ≈ 188 HK ≈ 458 HK 7.9 HK 15 HK ASTM E92 Durometers Indentor Shape & Extension Spring Force Cone Angle Orifice Diameter
New Berlin, WI, US
ASTM E92 CMC is stated as the repeatability as defined in ASTM E92 Indirect Verification of Rockwell & Rockwell Superficial Hardness Testers3 HRA: Low Medium High HRBW: Low Medium High HRC: Low
Glendale Heights, IL, US
ASTM E92 Heat Treat (Raw Material) AMS 27501 Impact Testing (Charpy and Izod) (-320 to 450) °F ASTM A370, E23; BS EN ISO 148-1; BS EN 10045-1 :2001 Metallographic Evaluation Alpha Case ASTM F136; SOP 02-11-S007 Case Depth AS
Charlotte, NC, US
ASTM E92 Metallographic Preparation ASTM E3 Field Metallographic Replicas ASTM E1351 Microetching ASTM E407 Grain Size ASTM E112 Microstructure of Graphite in Iron Castings ASTM A247
Corydon, IN, US
ASTM E92 using hardness test blocks Mass Determination 1 g 100 g 200 g 500 g 5 lb 10 lb 20 lb 50 lb 100 lb Up to 600 lb (600 to 1250) lb 64 µg 74 µg 95 µg 1 mg 0.73 mg 2 mg 8.1 mg 15 mg 0.17 g 0.2
Danville, VA, US
ASTM E92 Tension Testing of Metallic Materials ASTM E8/E8M Microetching Metals and Alloys ASTM E407 Macroetching Metals and Alloys ASTM E340 Charpy Impact ASTM E23/A370 Bend Testing AWS B4.0 Sec. 6 Metallographic Sampl
Madison, AL, US
ASTM E92 Indirect Verification of Microindentation Vickers3 (100 to 1000) HV (12 + 0.012X) HV ASTM E92 Indirect Verification of Hardness Brinell 10mm ball HBW 500kg 1000 kg
Allentown, PA, US
ASTM E92 Brinell Hardness (3000 kg) ASTM E10 Microhardness (HV 300g) ASTM E384 Rockwell Hardness (HRA, HRB, HRC) (15N) ASTM E18
Owatonna, MN, US
Parameter/Equipment Range CMC2 (±) Comments Scales & Balances3 (0.002 to 6.8) lb (6.8 to 50) lb (50 to 1000) lb (1001 to 5000) lb (5001 to 10 000) lb (0.000 040) lb (0.0022 + 0.0027W) lb 0.30 lb 1.6 lb 2.1 lb Verificat
West Boylston, MA, US
ASTM E92 Rockwell (A, B, C, E) ASTM A370, E18 Rockwell Superficial (15N, 30N, 15T, 30T) ASTM A370, E18
Saginaw, MI, US
ASTM E92 Torque Wrenches3 (4 to 1000) lbf·in (20 to 600) lbf·ft 0.5 % 0.5 % CDI Suretest 5000-ST Torque Wrenches (100 to 2000) lbf·ft 0.59 % CDI Computest Torque Transducer 0.5 ozf·in to 20
Paris, OH, US
ASTM E92 / E384 ASTM E92 / E384
Piedmont, SC, US
ASTM E92 & test blocks Brinell Hardness Testers 3 (200 to 399) HBW (400 to 600) HBW 1.6 HBW 8.0 HBW Indirect verification per ASTM E10 & test blocks Force – Testing Machines (Load Cells with Indicators), Dynamomete
Charlotte, NC, US
ASTM E92, E384 Knoop (100, 200, 300, 500, 1000) gf ASTM E92, E384 Impact (Charpy / (-320 to 450) oF) ASTM A370, E23; ISO 148-1 Metallography/Micrography on Ferrous and Nonferrous Materials Alpha Case GE P3TF19, P3TF32
Pompano Beach, FL, US
ASTM E92 Indirect Verification of Microindentation Vickers3 (100 to 1000) HV (12 + 0.012X) HV ASTM E92 Indirect Verification of Hardness Brinell 10mm ball HBW 500kg 1000 kg
Columbus, OH, US
ASTM E92 Vickers Micro Hardness (100, 200, 300, 500, 1000 gf) ASTM E384
Hunt Valley, MD, US
ASTM E92; ASTM E384; ASTM D2583; IPC-TM-650 (Method 2.4.27.2) Corrosion of Flux using Temperature/Humidity Chamber IPC-TM-650 (Method 2.6.15) Hydrolytic Stability/Temperature/Humidity Aging IPC-TM-650 (Methods 2.6.11 and 2.6.11.1);
Novi, MI, US
ASTM E92 using NIST Vickers or Knoop standard reference material (SRM) 1906, 1893, 1894a, 1895, and 1896. All other micro-indentation scales are traceable to the MPA or Sun-Tec hardness levels through laboratory standardizing machines.
Erie, PA, US
Test: Test Methods: Metallographic Evaluation: Preparation ASTM E3 Conductivity AMS 2658 Decarburization ASTM E1077, ASTM F2328 Case Depth SAE J423 Ferrite Rating AMS 2315; ASTM E562 Grain Size (Comparison Method Only) ASTM E112
Huntington Beach, CA, US
ASTM E92; ISO 6507-1 Corrosion Testing Alternate Immersion Stress Corrosion ASTM G38, ASTM G44, ASTM G47, ASTM G49 Copper Sulfate ASTM A380; MIL-STD-753 (Method 102) Exfoliation Corrosion ASTM G34 Humidity Testing AMS-QQ-P-35; AMS27
Showing labs 1–50 of 99. Use pagination below to see more.
American Association for Laboratory Accreditation (A2LA) is the primary accreditation body issuing ISO/IEC 17025 accreditation for testing laboratories in United States.
ISO/IEC 17025 is the international standard for the competence of testing and calibration laboratories. Accreditation to this standard provides independent confirmation that a laboratory operates a quality management system and is technically competent to produce valid results within its declared scope.